Alloynex makes castings for pump and valve OEMs from Jaipur, Rajasthan. A pump casing or valve body is a pressure part. It must hold pressure, resist the fluid, machine cleanly and pass the shell test the first time. So every enquiry starts with your service conditions, not the weight of the part.
Send your drawing for a technical review – info@alloynex.com
Parts we review for pump and valve OEMs
- Pumps: volute and split casings, suction and delivery covers, bearing housings, stuffing boxes, impellers, diffusers, wear rings, base and pedestal castings
- Valves: gate, globe, check and ball valve bodies, bonnets, covers, yokes, wedges and discs, end flanges, strainer bodies
Choose the grade by service, not by habit
The fluid, pressure and temperature decide the grade. This table is a buyer guide, not a supply list. Write your standard and grade on the drawing and agree them in writing at the technical review.
| Service | Common grade | Standard | Why it is chosen |
|---|---|---|---|
| Clean water, low pressure pumps and valves | Grey iron FG 200 / FG 260 (EN-GJL-250) | IS 210, EN 1561 | Good damping, easy to machine, sound in complex shapes |
| Water, irrigation, fire and municipal service, higher pressure or shock | SG iron SG 400/15, SG 500/7 (EN-GJS-400-15, EN-GJS-500-7) | IS 1865, EN 1563 | Much tougher than grey iron; resists cracking from water hammer |
| Process, steam, oil and general industrial valves | Carbon steel WCB / WCC | ASTM A216 | Weldable; the default body grade for steel valves |
| Cold service (LPG, refrigeration, cold climates) | Low-temperature steel LCB / LCC | ASTM A352 | Impact tested at minus 46 °C |
| High-temperature steam and power | Cr-Mo steel WC6 / WC9 | ASTM A217 | Holds strength and resists creep at high temperature |
| Corrosive fluids, chemicals, sea water | Stainless CF8 / CF8M, duplex grades | ASTM A351, ASTM A890 | Corrosion resistance – choose only after a fluid review |
For hot steam service, see our guide WC6 vs WC9 chrome-moly castings.
Key properties at a glance
Minimum values from the standards. Thick sections and test-bar rules apply – always check the standard named on your drawing.
| Grade | Min tensile (MPa) | Min yield (MPa) | Min elongation | Typical service limit |
|---|---|---|---|---|
| IS 210 FG 260 | 260 | – | – | Low pressure, ambient |
| IS 1865 SG 400/15 | 400 | 250 | 15 % | Water service, shock |
| IS 1865 SG 500/7 | 500 | 320 | 7 % | Higher strength, wear |
| ASTM A216 WCB | 485 to 655 | 250 | 22 % | About -29 to 425 °C |
| ASTM A216 WCC | 485 to 655 | 275 | 22 % | About -29 to 425 °C |
| ASTM A352 LCC | 485 to 655 | 275 | 22 % | Impact tested at -46 °C |
| ASTM A217 WC6 | 485 to 655 | 275 | 20 % | High temperature, up to about 595 °C |
Service limits are the usual ranges for valve bodies under ASME B16.34. Your design code and pressure-temperature rating decide the final limit.
Pressure-tight castings: what really matters
A pump or valve casting can look perfect and still leak under test. Leaks come from hidden shrinkage, gas porosity, sand or slag inclusions, and cold shuts in thin walls. These are the controls that keep a casting pressure-tight:
- Feeding and gating design – risers placed so heavy sections such as flanges and bosses solidify last and do not form shrinkage.
- Controlled chemistry – ask for the chemistry result of each heat, so strength and weldability stay inside the grade.
- Clean metal – slag removal, filters and calm pouring to keep inclusions out of the wall.
- Sound sand and cores – correct core venting so gas does not get trapped in the casting.
- Heat treatment to the grade – normalising, or normalising and tempering, for steel grades; annealing for SG iron where the drawing asks for it.
- No hidden repairs – any weld repair on a pressure casting must follow a qualified procedure and be recorded, as the standard requires.
Read more: Common casting defects and how we prevent them | Heat treatment of castings
Inspection and NDT for valve and pump castings
Valve buyers often name these standards on the drawing or purchase order:
| Check | Common standard | What it finds |
|---|---|---|
| Visual surface check | MSS SP-55 | Surface defects, against reference photos |
| Magnetic particle testing (MPT) | MSS SP-53, ASTM E709 | Surface and near-surface cracks in steel and iron |
| Dye penetrant testing (DPT) | MSS SP-93 | Surface cracks, also in stainless grades |
| Radiography (RT) | MSS SP-54, ASTM E446 / E186 | Internal shrinkage, porosity and inclusions |
| Ultrasonic testing (UT) | ASTM A609 | Internal defects in thick walls |
| Shell (hydrostatic) test | API 598, ISO 5208, EN 12266-1 | Leaks through the body wall – usually done by the valve maker after machining |
| Chemistry and mechanical test | Grade standard, EN 10204 certificate | Proof that the heat meets the grade |
See also: EN 10204 test certificates explained
Built for machining
Pump and valve castings are always machined – seats, bores, flange faces and threads. A good casting saves you time on the shop floor:
- Machining allowance agreed on the drawing before the pattern is made
- Location points and datum pads marked for the first machining setup
- Hardness kept inside the grade range, so tools last and seats finish well
- Flange faces and seat areas kept clean of sand and scale
Read more: Machining allowance on castings
Related grades and guides
- SG iron vs grey cast iron – which one for your part
- Steel vs alloy steel castings
- Valve body castings
- IS 210 FG 200 vs FG 260 vs FG 300
What to send for a technical review
To review a pump or valve casting enquiry well, please send:
- Drawing (PDF or STEP), with machining marked if known
- Part type and the pump or valve it goes into
- Material standard and grade (for example ASTM A216 WCB, IS 1865 SG 500/7)
- Fluid, design pressure and temperature, or the pressure class (for example Class 150, PN 16)
- Weight per piece and annual quantity, with batch size
- Tests and certificates needed (NDT, radiography level, certificate type, third-party inspection)
- Delivery city or country, and your timeline
Send your drawing for a technical review. Email info@alloynex.com or use the enquiry form with drawing upload. Our team checks grade, wall thickness and test needs against your service before anything else.
FAQ
Which material is best for a pump casing?
For clean water at low pressure, grey iron such as IS 210 FG 260 is common. For higher pressure, shock or water hammer, SG iron such as IS 1865 SG 400/15 or SG 500/7 is tougher. For hot, hydrocarbon or high-pressure service, cast steel such as ASTM A216 WCB is usual. Corrosive fluids need a stainless or duplex grade chosen after a fluid review.
What is WCB material in valves?
WCB is a cast carbon steel grade in ASTM A216. It has a minimum tensile strength of 485 MPa and a minimum yield strength of 250 MPa. It is weldable and is the most common body and bonnet grade for steel gate, globe and check valves.
What is the difference between WCB and WCC?
Both are ASTM A216 cast carbon steels. WCC has a higher minimum yield strength, 275 MPa against 250 MPa for WCB, because its manganese limit is higher. WCC is used where a little more strength is needed at the same wall thickness.
When should I choose LCB or LCC instead of WCB?
Choose ASTM A352 LCB or LCC when the valve or pump will see temperatures below about minus 29 °C, such as LPG, refrigeration or cold-climate service. These grades are impact tested at minus 46 °C, so they do not turn brittle in the cold.
Why do valve castings leak in the shell test?
Most leaks come from hidden shrinkage, gas porosity, inclusions or cold shuts in the wall. Good feeding design, clean metal, vented cores and controlled chemistry prevent them. Radiography or ultrasonic testing on critical areas finds them before machining.
Which NDT standards apply to valve castings?
Common ones are MSS SP-55 for visual checks, MSS SP-53 for magnetic particle testing, MSS SP-93 for dye penetrant testing and MSS SP-54 for radiography. The shell test is usually done to API 598, ISO 5208 or EN 12266-1. Your drawing or purchase order should name the standard and the acceptance level.