For most grey iron castings, choose IS 210 FG 200 for lightly loaded parts that need easy machining, FG 260 for pump bodies, housings and machine parts under moderate load, and FG 300 only where the drawing needs higher strength and wear resistance. The number in each grade is its minimum tensile strength in MPa: FG 200 = 200 MPa, FG 260 = 260 MPa and FG 300 = 300 MPa, measured on a separately cast test bar.
This guide explains FG 200 vs FG 260 vs FG 300 in simple words. It is written for design engineers, buyers and QA teams who must write the right grey iron grade on a drawing. It covers what the grade codes mean, how the three grades differ, how to choose, and what tests to ask for.
What do FG 200, FG 260 and FG 300 mean in IS 210?
IS 210 is the Indian standard for grey iron castings. “FG” stands for flake graphite, because the carbon in grey iron forms thin graphite flakes. The number after FG is the minimum tensile strength in megapascals (MPa, the same as N/mm²).
The strength is not measured on the casting itself. It is measured on a separately cast test bar, poured from the same melt. This matters, because a thick casting cools slowly and can be weaker than the bar. A thin casting cools fast and can be harder than the bar.
IS 210 also has other grades, such as FG 150, FG 220, FG 350 and FG 400. FG 200, FG 260 and FG 300 are the three that buyers compare most often.
FG 200 vs FG 260 vs FG 300: spec table
The table shows the key values for the three grades. Tensile values are IS 210 minimums. Hardness ranges are typical guidance only, so always state the hardness you need on your drawing.
| Property | FG 200 | FG 260 | FG 300 |
|---|---|---|---|
| Min. tensile strength (IS 210, test bar) | 200 MPa | 260 MPa | 300 MPa |
| Typical hardness (BHN, approx.) | 160 to 220 | 180 to 230 | 180 to 250 |
| Matrix (typical) | Ferrite and pearlite | Mostly pearlite | Pearlite, finer graphite |
| Nearest EN 1561 grade | EN-GJL-200 | EN-GJL-250 | EN-GJL-300 |
| Nearest ASTM A48 class | Class 30 | Class 35 to 40 | Class 45 |
Equivalent grades are close, not exact. If your drawing uses an EN or ASTM grade, keep that grade on the drawing and confirm the match with your foundry.
How are the three grades different in real use?
A higher FG number means more strength, but it also changes other things. As the grade goes up, the iron usually has finer graphite flakes and more pearlite. That gives more strength and wear resistance, but slightly less damping and a little harder machining.
| Point | FG 200 | FG 260 | FG 300 |
|---|---|---|---|
| Strength | Good for light load | Good for moderate load | Highest of the three |
| Vibration damping | Best | Very good | Good |
| Machinability | Easiest | Easy | Fair, a little slower |
| Wear resistance | Moderate | Good | Very good |
| Sensitivity to thin walls | Low | Medium | Higher risk of hard edges (chill) |
| Typical parts | Covers, bases, counterweights, light housings | Pump bodies, motor housings, valve parts, brake drums | Heavy housings, machine tool beds, cylinder-type parts |
All grey iron grades have low ductility. They do not bend before breaking. If the part takes shock load, impact or bending, grey iron of any grade may not be right. In that case read our guide on SG iron vs grey cast iron.
How to choose between FG 200, FG 260 and FG 300
Use these steps. They take a few minutes and prevent most grade mistakes.
- Check the load. Light or no load: start with FG 200. Moderate working load or pressure: FG 260. High load or high stress: FG 300.
- Check for shock. If the part takes impact or bending, grey iron is a poor choice. Look at an SG iron grade instead.
- Check the wall thickness. Thick walls lower the strength in the casting. Thin walls in a high grade can form hard edges. Tell your foundry the thinnest and thickest sections.
- Check wear and sliding. Slideways, cylinder bores and wear faces often need FG 260 or FG 300.
- Check machining. If the part has a lot of machining and only light load, FG 200 saves tool life and time.
- Write it clearly. Put the standard and grade on the drawing, for example “Grey iron to IS 210 FG 260”, plus hardness range and tests.
Common mistakes when ordering grey iron grades
- Writing only “CI” or “cast iron”. This does not name a grade. Always write IS 210 and the FG number.
- Choosing FG 300 “to be safe”. A higher grade is not always better. It can machine slower and form hard edges on thin walls.
- Expecting the casting to match the test bar. Heavy sections can test lower than the bar. Ask for hardness on the casting if this matters.
- Ignoring stress relief. Large or precise parts may move during machining. Ask for stress relieving if the part must stay stable.
Which tests prove the grade?
A grade is proven by tests, not by the name on a label. For FG 200, FG 260 or FG 300 castings, buyers usually ask for:
- Chemical analysis of each melt (carbon, silicon, manganese, sulphur, phosphorus).
- Tensile test on a separately cast test bar, as IS 210 describes.
- Brinell hardness on the casting or the test bar.
- Microstructure check of graphite form and matrix, when the part is critical.
- Dimensional report against the drawing, and a test certificate such as EN 10204 3.1, linked by heat number.
Also mark machined faces and stock on the drawing. Our guide on machining allowance on castings explains how much to keep.
Grey iron grades at Alloynex Foundries
Alloynex Foundries, Harmada, Jaipur, makes grey iron castings to the buyer’s drawing. Name the IS 210 grade (for example FG 200 or FG 260) on the drawing. If your drawing names FG 300 or another grade, send it for a technical review and our team will confirm the grade, pattern, machining stock and tests before work starts. We work under ISO 9001, ISO 14001 and ISO 45001 systems. See our casting services and the castings buyer guide for OEMs.
Which iron grade suits agricultural machinery castings in Hanumangarh and Sri Ganganagar?
Last updated: 14 November 2026
For farm machinery made in Hanumangarh, most grey iron parts such as gearbox covers, pulleys, brackets and counterweights are ordered in IS 210 FG 200 or FG 260. Parts that take shock, such as hubs and loaded housings, often move to SG iron to IS 1865, such as SG 500/7. Alloynex Foundries casts both to drawing.
Agricultural casting grade guide (general education)
| Typical farm machinery part | Load in service | Grade often specified | Key check |
|---|---|---|---|
| Gearbox cover, side cover | Low, static | IS 210 FG 200 | Hardness, dimensions |
| Pulley, flywheel | Rotating, steady | IS 210 FG 260 | Balance faces, hardness |
| Counterweight, bracket | Static weight | IS 210 FG 150 or FG 200 | Weight, dimensions |
| Wheel hub, loaded bracket | Shock and vibration | IS 1865 SG 450/10 or SG 500/7 | Tensile, elongation, nodularity |
| Gearbox housing under shock | Gear load plus field shock | IS 1865 SG 500/7 | Tensile, nodularity, dimensional report |
Selection steps for agri buyers
- List how the part is loaded in the field: steady, rotating or shock.
- Use grey iron FG 200 or FG 260 where the load is steady.
- Use SG iron where a hit from soil, stone or a sudden stop can crack the part.
- Write the grade and standard on the drawing, not just “CI” or “SG”.
- Ask for test results traceable to the heat, with an EN 10204 3.1 certificate.
- Approve samples, including fit and machining, before lot orders.
FG 200 vs FG 260 vs SG 500/7 for farm machinery
| Point | FG 200 | FG 260 | SG 500/7 |
|---|---|---|---|
| Min. tensile strength (MPa) | 200 | 260 | 500 |
| Elongation | Very low | Very low | About 7 percent minimum |
| Shock in the field | Poor | Fair | Good |
| Machining | Very easy | Easy | Good |
| Best for | Covers, light housings | Pulleys, loaded covers | Hubs, shock-loaded housings |
Rule of thumb: if a cracked part would stop a tractor in the field, specify SG iron. Grey iron is right for covers and steady loads.
Quick answers for Hanumangarh buyers
Do you supply castings for agricultural machinery makers in Hanumangarh?
Yes. Alloynex Foundries makes grey iron and SG iron castings to drawing and serves buyers across Rajasthan, including Hanumangarh and Sri Ganganagar.
Is “CI casting” enough on a purchase order?
No. Write the full grade, such as IS 210 FG 260 or IS 1865 SG 500/7. Without a grade, test results cannot be checked.
हनुमानगढ़ में कृषि मशीन के लिए कौन सा कास्टिंग ग्रेड लें?
कवर और पुली जैसे पार्ट्स के लिए IS 210 FG 200 या FG 260 ग्रे आयरन ठीक है। झटके वाले पार्ट्स, जैसे हब, के लिए IS 1865 SG 500/7 एसजी आयरन लें। एलॉयनेक्स फाउंड्रीज़, जयपुर। ड्रॉइंग info@alloynex.com पर भेजें।
Service area: Hanumangarh, Sangaria, Rawatsar, Nohar, Bhadra, Pilibanga, Sri Ganganagar and Suratgarh, served from Harmada, Jaipur.
Read SG iron vs grey cast iron and the castings buyer guide for Rajasthan. Request a metallurgy consultation: info@alloynex.com.
FAQs
What is the tensile strength of FG 200, FG 260 and FG 300?
As per IS 210, the minimum tensile strength is 200 MPa for FG 200, 260 MPa for FG 260 and 300 MPa for FG 300, measured on a separately cast test bar.
Is FG 260 better than FG 200?
FG 260 is stronger and wears better. FG 200 machines more easily and damps vibration better. The better grade is the one that matches the load on your part.
When should I choose FG 300?
Choose FG 300 when the part carries high stress or needs good wear resistance, such as heavy housings or machine tool beds, and the walls are not too thin.
What is the EN equivalent of FG 260?
The nearest EN 1561 grade is EN-GJL-250. It is close but not identical, so confirm the match on your drawing.
FG 200, FG 260 और FG 300 में क्या अंतर है?
IS 210 के अनुसार FG 200 की न्यूनतम टेन्साइल स्ट्रेंथ 200 MPa, FG 260 की 260 MPa और FG 300 की 300 MPa है। हल्के पार्ट के लिए FG 200, पंप बॉडी और हाउसिंग के लिए FG 260, और ज़्यादा लोड वाले पार्ट के लिए FG 300 चुनें।
ड्रॉइंग पर ग्रे आयरन ग्रेड कैसे लिखें?
ड्रॉइंग पर स्टैंडर्ड और ग्रेड दोनों लिखें, जैसे “IS 210 FG 260″। साथ में हार्डनेस, मशीनिंग स्टॉक और ज़रूरी टेस्ट भी लिखें। अपनी ड्रॉइंग info@alloynex.com पर भेजें।
Send your drawing for a technical review
Not sure if your part needs FG 200, FG 260 or FG 300? Email your drawing, load details, quantity and test needs to info@alloynex.com or request a metallurgy consultation.
Last updated: 13 November 2026
Related: FG 200, FG 260 and SG iron grade table for Nagaur and Sirohi buyers
अलवर में ग्रे आयरन कास्टिंग कौन सप्लाई करता है? (Who supplies grey iron castings to Alwar buyers?)
Quick answer: Alloynex Foundries, Harmada, Jaipur, makes grey iron castings to the buyer’s drawing for buyers in Alwar, MIA Alwar, Bhiwadi and Khairthal-Tijara. Name the IS 210 grade (for example FG 200 or FG 260) on the drawing. Each order starts with a drawing review, and the grade is checked by chemistry and a tensile test bar. Send your drawing to info@alloynex.com for a technical review.
संक्षिप्त उत्तर: Alloynex Foundries, जयपुर, IS 210 के FG 200 और FG 260 जैसे ग्रेड में ग्रे आयरन कास्टिंग आपकी ड्रॉइंग के अनुसार बनाता है। अलवर, MIA अलवर, भिवाड़ी और खैरथल-तिजारा के खरीदार अपनी ड्रॉइंग info@alloynex.com पर तकनीकी समीक्षा के लिए भेज सकते हैं।
Alwar district and the Bhiwadi belt run pump, motor, auto component, machine tool and agricultural equipment plants. Most of their cast parts are housings, covers, bases, pulleys, brake drums and gear blanks. Grey iron suits these because it machines easily and damps vibration.
| IS 210 grade | Min. tensile strength (MPa) | Typical part for Alwar and Bhiwadi plants | Ask on the certificate |
|---|---|---|---|
| FG 150 | 150 | Covers, counterweights, non-load parts | Chemistry, test bar tensile |
| FG 200 | 200 | Pump and motor housings, pulleys, machine bases | Chemistry, tensile, hardness |
| FG 260 | 260 | Gear blanks, brake drums, cylinder parts, wear parts | Chemistry, tensile, hardness |
| FG 300 | 300 | Heavily loaded machine tool parts | Chemistry, tensile, hardness, microstructure if agreed |
Tensile values are the minimum for the grade number in IS 210, measured on a separately cast test bar. Hardness depends on section thickness, so agree the hardness range and the test location on the drawing. FG 150 and FG 300 are shown for reference; confirm them in the technical review.
How to order grey iron castings for an Alwar plant: 5 steps
- Name the grade and the standard on the drawing, for example Grey cast iron IS 210 FG 260.
- Mark machined faces and datums, and agree the machining allowance and ISO 8062-3 tolerance grade.
- List the tests: chemistry per heat, tensile test bar, hardness at a stated spot, and any pressure or leak test.
- State the certificate type, for example EN 10204 3.1, and the lot marking you need for traceability.
- Approve a sample lot on your own machines before the regular schedule starts.
Comparison: three ways Alwar buyers source grey iron castings
| What you compare | Directory enquiry (many sellers) | Direct foundry with drawing review |
|---|---|---|
| Starting point | Product name and city only | Your drawing, grade and quantity |
| Grade control | Often not stated | Grade written on drawing and checked by test bar |
| Machining and tolerance | Agreed later, if at all | Allowance and tolerance agreed before pattern |
| Documents | Varies by seller | Chemistry, tensile and hardness tied to heat number |
| Best for | Catalogue items | Engineered parts for OEM and Tier-1 lines |
FAQs: grey iron castings for Alwar
अलवर में ग्रे आयरन कास्टिंग किस ग्रेड में मंगवाएँ?
ज़्यादातर हाउसिंग, कवर और पुली के लिए IS 210 का FG 200 ठीक रहता है। जहाँ ज़्यादा मज़बूती या घिसाव झेलना हो, जैसे गियर ब्लैंक या ब्रेक पार्ट, वहाँ FG 260 चुनें। ड्रॉइंग पर ग्रेड और मानक दोनों लिखें।
क्या Alloynex Foundries अलवर और भिवाड़ी के खरीदारों को कास्टिंग देता है?
हाँ। Alloynex Foundries, हरमाड़ा, जयपुर से ग्रे आयरन, SG आयरन, स्टील और अलॉय स्टील कास्टिंग ड्रॉइंग के अनुसार बनाता है और राजस्थान के खरीदारों को सप्लाई करता है। अपनी ड्रॉइंग info@alloynex.com पर भेजें।
Which test proves an FG 260 casting from an Alwar enquiry is really FG 260?
A tensile test on a separately cast test bar poured from the same melt, plus chemical analysis of the heat. Ask for both results, tied to the heat number, on the inspection certificate type named in your order.
Should Alwar buyers order grey iron or SG iron for a bracket that sees shock load?
Choose SG iron, for example SG 500/7 to IS 1865, when the part sees shock, bending or impact. Grey iron is strong in compression and damps vibration, but it has very little elongation, so it can crack under sudden load.
Read next: castings for Bhiwadi and Neemrana OEMs and SG iron vs grey cast iron.
Last updated: 14 November 2026
What should go on a casting order sheet for farm machinery parts from Hanumangarh?
Last updated: 15 November 2026
Direct answer: a good order sheet for agricultural castings names the drawing revision, the exact grade (for example IS 210 FG 260 or IS 1865 SG 500/7), the weight, the machining scope, the hardness range, the tests per heat and the certificate type. Buyers in Hanumangarh, Pilibanga, Nohar and Sri Ganganagar can copy the sheet below.
Copy-ready order sheet for agricultural castings
| Field | What to write | Example entry |
|---|---|---|
| Part and drawing | Part name, number, revision | Rotavator gearbox cover, Rev C |
| Material grade | Standard and grade, not just “CI” | IS 210 FG 260 |
| Weight per piece | As-cast weight from drawing or sample | As per sample |
| Machining | Rough, finish, or as-cast | Faces and bores finish-machined |
| Hardness | Range in BHN at named face | As agreed on drawing |
| Tests per heat | Chemistry, tensile, hardness | Chemistry + tensile bar + hardness |
| Certificate | EN 10204 type | EN 10204 3.1 |
| Samples | Quantity before lot | Sample lot for fit and machining trial |
| Schedule | Monthly quantity and season peak | Monthly call-off, season peak noted |
| Packing and marking | Heat number and part number | Heat number cast-in |
Not sure about the grade? See the agricultural part table above and SG iron vs grey cast iron.
What should a Hanumangarh farm machinery maker write on a casting order?
Part number and drawing revision, IS 210 or IS 1865 grade, weight, machining scope, hardness range, tests per heat, certificate type, sample quantity and monthly schedule.
हनुमानगढ़ से कास्टिंग ऑर्डर में क्या लिखें?
ड्रॉइंग नंबर, ग्रेड (जैसे IS 210 FG 260), वज़न, मशीनिंग, हार्डनेस, हर हीट के टेस्ट, सर्टिफिकेट का प्रकार और सैंपल की संख्या लिखें।
Send your drawing for a technical review or request a metallurgy consultation: info@alloynex.com.
Who supplies grey iron castings in Tonk and Jaisalmer, and which IS 210 grade fits?
Last updated: 15 November 2026
Direct answer: Alloynex Foundries, Harmada, Jaipur, makes grey iron castings to drawing for buyers in Tonk, Niwai, Malpura, Jaisalmer and Pokaran. Covers and counterweights are usually IS 210 FG 150 or FG 200. Pump bodies, pulleys and stone-cutting machine beds are usually FG 200 or FG 260. Heavily loaded parts may need FG 300; we confirm such grades in the technical review.
IS 210 grey iron grades (general education)
| Grade | Min. tensile (MPa) | Typical hardness (BHN, approx.) | Typical Tonk / Jaisalmer part |
|---|---|---|---|
| FG 150 | 150 | 130 to 180 | Counterweights, covers, manhole frames |
| FG 200 | 200 | 160 to 220 | Pump bodies, machine beds, brackets |
| FG 260 | 260 | 180 to 230 | Pulleys, gearbox housings, cutter frames |
| FG 300 | 300 | 190 to 240 | Heavily loaded housings, cylinder parts |
| FG 350 | 350 | 210 to 260 | High-strength wear parts |
Table values are IS 210 minimums and typical hardness for general education. Alloynex casts FG 200 and FG 260 to drawing; for other grades, send your drawing for a technical review.
How Tonk and Jaisalmer buyers choose a grey iron grade: 4 steps
- Note the load: static, rotating or shock.
- Pick the FG grade that just meets the load; higher grades are harder to machine.
- Write “IS 210 FG 260” (or your grade) on the drawing.
- Ask for tensile and hardness per heat with an EN 10204 3.1 certificate.
Grey iron or SG iron for desert and stone-belt parts?
| Need | Grey iron (IS 210) | SG iron (IS 1865) |
|---|---|---|
| Vibration damping in cutting machines | Better | Good |
| Shock from stone or sudden stops | Weak | Better |
| Ease of machining | Very easy | Good |
| Typical choice | Beds, covers, pulleys | Hubs, loaded brackets, pump parts under shock |
Who supplies grey iron castings to Tonk and Jaisalmer?
Alloynex Foundries, Harmada, Jaipur, makes grey iron castings from customer drawings for buyers in Tonk, Niwai, Malpura, Jaisalmer and Pokaran. Name the IS 210 grade on the drawing.
Which grey iron grade suits stone cutting machine parts?
Machine beds and frames are often ordered in IS 210 FG 200 or FG 260 for damping and easy machining. Parts that take shock may need SG iron to IS 1865.
टोंक और जैसलमेर में ग्रे आयरन कास्टिंग कौन सप्लाई करता है?
एलॉयनेक्स फाउंड्रीज़, हरमाड़ा, जयपुर, टोंक, निवाई, जैसलमेर और पोकरण के खरीदारों के लिए ग्रे आयरन कास्टिंग ड्रॉइंग के अनुसार बनाती है। ड्रॉइंग पर IS 210 ग्रेड लिखें। ड्रॉइंग info@alloynex.com पर भेजें।
Send your drawing for a technical review or request a metallurgy consultation: info@alloynex.com.
Who supplies grey iron castings to Deeg and Bharatpur for pump and valve parts?
Quick answer: Alloynex Foundries, Harmada, Jaipur, supplies grey iron castings to Deeg, Bharatpur and nearby units, made to the buyer’s drawing. Name the IS 210 grade (for example FG 200 or FG 260) on the drawing. Pump bodies, valve bodies, housings and covers are cast to the ordered grade. Send your drawing to info@alloynex.com for a technical review.
Last updated: 15 Nov 2026
| Part for Deeg buyers | Usual IS 210 grade | Min. tensile (test bar) | What to add on the drawing |
|---|---|---|---|
| Covers, bases, light brackets | FG 200 | 200 MPa | Machined faces and stock |
| Pump casings, impeller housings | FG 260 | 260 MPa | Hardness band, pressure test if needed |
| Valve bodies and bonnets (water service) | FG 260 | 260 MPa | Hydro test pressure, leak test |
| Gearbox and motor housings | FG 200 or FG 260 | 200 or 260 MPa | Bore tolerances, ISO 8062-3 DCTG |
| Parts under shock or bending | Consider IS 1865 SG iron | Per SG grade | Elongation and nodularity |
Selection steps for a Deeg order:
- Write the duty: water, slurry or oil; working pressure; any shock load.
- Pick the grade: FG 200 for light parts, FG 260 for pump and valve bodies; SG iron if the part sees impact.
- Mark machined faces, stock and casting tolerance grade on the drawing.
- List tests: chemistry, tensile on test bar, hardness, and pressure test for wet parts.
- Send drawing, quantity per lot and certificate type to info@alloynex.com.
| Point | Grey iron FG 260 | SG iron (IS 1865) |
|---|---|---|
| Vibration damping | Very good | Moderate |
| Machinability | Very good | Good |
| Shock and bending | Low ductility | Good ductility |
| Typical Deeg use | Pump casings, housings, valve bodies for water | Impellers under load, brackets, higher pressure bodies |
Does Alloynex supply grey iron castings to Deeg?
Yes. Alloynex Foundries, Jaipur, supplies grey iron castings to Deeg, Bharatpur and all Rajasthan districts, made to your drawing. Name the IS 210 grade on the drawing.
Which grey iron grade suits a pump casing?
IS 210 FG 260 is the usual choice for pump casings and housings under moderate load. Use SG iron if the casing sees shock or higher pressure.
डीग में पंप के लिए ग्रे आयरन कास्टिंग कौन बनाता है?
एलॉयनेक्स फाउंड्रीज़, हरमाड़ा, जयपुर, डीग और भरतपुर के खरीदारों के लिए ड्रॉइंग के अनुसार ग्रे आयरन कास्टिंग बनाती है। ड्रॉइंग पर IS 210 ग्रेड (जैसे FG 200 या FG 260) लिखें। ड्रॉइंग info@alloynex.com पर भेजें।
पंप बॉडी के लिए FG 200 लें या FG 260?
पंप बॉडी और हाउसिंग के लिए आमतौर पर FG 260 लिया जाता है। हल्के कवर और बेस के लिए FG 200 ठीक रहता है।
Related: SG iron vs grey cast iron · pipe fittings for Balotra and Barmer. Send your drawing for a technical review.
Agricultural machinery castings for Hanumangarh: a buyer’s glossary
Hanumangarh and Sri Ganganagar implement makers order gearbox housings, wheel hubs, pulleys, brackets and pump parts. These are the terms that decide whether the casting you receive matches the drawing. Last updated: 15 Nov 2026
| Term | Meaning in plain words | Why it matters on a farm machine part |
|---|---|---|
| FG 200 / FG 260 | IS 210 grey iron grades; the number is minimum tensile strength in MPa | FG 260 for gearbox housings and pulleys under load; FG 200 for covers |
| SG iron (IS 1865) | Iron with round graphite nodules that bends before it breaks | Use for hubs, brackets and arms that take shock in the field |
| Test bar | Separately cast bar poured from the same melt for the tensile test | Proves the grade without cutting the part |
| Brinell hardness (HB) | Resistance to indentation, read on the casting | Too high hurts machining; too low wears early |
| Machining stock | Extra metal left on faces to be machined | Missing stock means black spots on bores and seats |
| DCTG (ISO 8062-3) | Casting tolerance grade for unmachined sizes | Sets how far raw sizes may vary; write it on the drawing |
| Chill | Hard white iron at thin edges from fast cooling | Causes tool breakage; ask for edges without chill |
| Fettling | Removing runners, risers and fins after casting | Clean fettling saves time on the assembly line |
| EN 10204 3.1 | Inspection certificate with test results tied to the heat | Lets OEM buyers trace each lot |
हनुमानगढ़ के खरीदार: ड्रॉइंग पर “IS 210 FG 260” जैसा पूरा ग्रेड, हार्डनेस और मशीनिंग स्टॉक लिखें और info@alloynex.com पर भेजें।
Related: pipe fittings for Balotra and Barmer · ERW pipe for Bundi · SG iron pump castings for Phalodi. Send your drawing for a technical review.
Related: FG 150 and FG 200 grey iron for counterweight castings in Bhilwara, grey iron, SG iron and WCB valve body castings in Jaipur, steel castings for Tonk and high manganese IS 276 castings
Related: grey iron compressor body and cylinder castings in Jaipur, SG iron hydraulic castings for Bhiwadi OEMs, झुंझुनू में पाइप फिटिंग्स और फ्लैंज and राजस्थान में ग्रे आयरन और एसजी आयरन कास्टिंग सप्लायर (हिंदी गाइड).
FG 200, FG 260 or FG 300? A yes/no decision tree for IS 210 grey iron
Short answer: start at FG 200 and move up only when the part needs it. Choose FG 260 when the part carries real load, needs better wear on sliding faces or is a pump or motor body. Choose FG 300 for heavy machine tool parts, cylinder-type parts and highly loaded housings. Thick sections lose strength, so check wall thickness first. Last updated: 16 Nov 2026
| Question | If yes | If no |
|---|---|---|
| Q1. Is the part a cover, guard, base plate or counterweight with little load? | FG 200 (FG 150 for non-load parts if the drawing allows) | Go to Q2 |
| Q2. Is it a pump body, motor housing, flywheel, brake drum or gearbox housing? | FG 260 | Go to Q3 |
| Q3. Is it a machine tool bed, slideway, cylinder-type part or heavily loaded housing? | FG 300 | Go to Q4 |
| Q4. Is the main wall thicker than about 50 mm? | Go one grade higher, or ask for strength proof on a test block of matching section | Keep the grade from Q1 to Q3 |
| Q5. Does the part take shock or impact loads? | Do not use grey iron; consider IS 1865 SG iron | Grey iron is fine |
Every IS 210 grade number is the minimum tensile strength in MPa on a separately cast 30 mm test bar: 200, 260 and 300 MPa. Hardness is a quick check, not proof of grade.
हिंदी त्वरित उत्तर: FG 200, FG 260 या FG 300 कौन सा चुनें?
हल्के लोड वाले कवर और बेस के लिए FG 200, पंप बॉडी, मोटर हाउसिंग, फ्लाईव्हील और ब्रेक ड्रम के लिए FG 260, और भारी मशीन टूल पार्ट्स के लिए FG 300 चुनें। झटके वाले लोड पर ग्रे आयरन की जगह SG आयरन लें।
Related: flywheel castings for Alwar buyers and grey iron castings for Sawai Madhopur. Send your drawing for a technical review to info@alloynex.com, or request a metallurgy consultation on the grade.