Quick answer: Use IS 2062 (grades E250 to E450, with impact quality A, BR, B0 or C) when steel must carry load in a welded or bolted structure. Use IS 1079 (HR1 to HR4) when hot rolled sheet, plate or strip must be bent, pressed or drawn. IS 2062 is chosen for strength; IS 1079 is chosen for forming.
Both standards come from the Bureau of Indian Standards (BIS) and both cover hot rolled steel, so they are often mixed up on drawings and purchase orders. This guide explains the difference in simple words, gives a grade table, a decision matrix and a five-step way to write the right line on your drawing. It is written for design engineers, QA heads and buyers in Jaipur, Rajasthan and across India.
What is the difference between IS 2062 and IS 1079?
IS 2062 is the Indian standard for hot rolled medium and high tensile structural steel. It covers plates, strips, sheets, flats, bars and sections used in frames, bridges, machine bases, tanks and other load-bearing work. Each grade name tells you the minimum yield strength: E250 means 250 MPa, E350 means 350 MPa.
IS 1079 is the Indian standard for hot rolled carbon steel sheet, plate and strip. Its grades, from HR1 (commercial quality) to HR2, HR3 and HR4 (drawing, deep drawing and extra deep drawing qualities), are chosen for how well the steel bends, presses and draws without cracking. It is the usual choice for pressed covers, panels, enclosures, ducting and formed brackets.
IS 2062 vs IS 1079: comparison table
| Point | IS 2062 | IS 1079 |
|---|---|---|
| Full title (short) | Hot rolled medium and high tensile structural steel | Hot rolled carbon steel sheet, plate and strip |
| Main purpose | Strength for load-bearing, welded or bolted structures | Formability for bending, pressing and drawing |
| Product forms | Plates, strips, sheets, flats, bars, angles, channels, beams | Sheet, plate and strip (coil or cut length) |
| Grade names | E250, E275, E300, E350, E410, E450 and higher | HR1, HR2, HR3, HR4 and related grades |
| What the grade guarantees | Minimum yield and tensile strength, elongation, impact level | Chemistry limits and forming properties for the quality level |
| Impact test | Quality A (none), BR (room temperature), B0 (0 °C), C (minus 20 °C) | Not the basis of grade choice |
| Weldability | Controlled carbon equivalent for welding | Low carbon, weldable for sheet work |
| Typical parts | Machine bases, frames, columns, gussets, tank shells, crane girders | Covers, panels, enclosures, ducting, pressed brackets |
IS 2062 grades: strength at a glance
Values below are the minimum figures for thinner sections as given in IS 2062:2011. Yield strength drops a little as thickness goes up, so always read the table in the standard for your thickness.
| IS 2062 grade | Min. yield strength (MPa, thin sections) | Min. tensile strength (MPa) | Min. elongation (%) |
|---|---|---|---|
| E250 | 250 | 410 | 23 |
| E275 | 275 | 430 | 22 |
| E300 | 300 | 440 | 22 |
| E350 | 350 | 490 | 22 |
| E410 | 410 | 540 | 20 |
| E450 | 450 | 570 | 20 |
A full grade on a drawing adds the impact quality, for example IS 2062 E250 BR or IS 2062 E350 B0. Writing only “IS 2062” leaves the grade open and invites the wrong material.
IS 1079 grades: forming quality at a glance
| IS 1079 grade | Quality level | Typical use |
|---|---|---|
| HR1 | Commercial quality | General sheet work, simple bends |
| HR2 | Drawing quality | Moderate pressing and forming |
| HR3 | Deep drawing quality | Deeper pressed shapes |
| HR4 | Extra deep drawing quality | Severe draws, complex pressings |
For IS 1079 the key is matching the quality level to how hard the part is formed. A higher drawing quality has tighter limits on carbon and other elements so the sheet can stretch more in the press.
Grade selector: which standard and grade should you specify?
- Does the part carry the main load in a welded or bolted structure? Yes: specify IS 2062 and go to step 2. No: go to step 3.
- Pick the IS 2062 strength and impact level. E250 BR suits general frames, machine bases and platforms; E350 BR suits higher design stress. Use B0 for service near 0 °C and C for service near minus 20 °C. Tank shells and girders take the grade from the design.
- Is the part pressed or formed from sheet, plate or strip? Specify IS 1079: HR1 for simple bends, HR2 for moderate pressing, HR3 for deeper draws and HR4 for severe or complex pressings.
- Is the part both formed and loaded? Ask for a design review. The load usually decides, so the answer is often IS 2062 with a forming check.
How to write the steel on your drawing: 5 steps
- Decide the job of the part: carry load (go to IS 2062) or be formed (go to IS 1079).
- Write the full grade: for example IS 2062 E350 BR, or IS 1079 HR2. Add the edition if your customer asks.
- Write the product form and size: plate, sheet, strip, flat or section, with thickness, width and length.
- List the tests: chemistry, tensile, elongation, bend, and impact at the stated temperature for IS 2062 B0 or C grades.
- Name the certificate: for example EN 10204 3.1 mill test certificate with heat number. Send the drawing for a technical review.
Common mistakes with IS 2062 and IS 1079
- Writing “MS plate” with no standard or grade.
- Ordering IS 1079 sheet for a welded load-bearing frame.
- Writing IS 2062 E250 without the impact quality (A, BR, B0 or C).
- Accepting a certificate with a different grade or no heat number.
- Using an old grade name, such as Fe 410 WA, without checking the current E-grade equivalent.
In simple words: IS 2062 is for strength, IS 1079 is for shape. If a part needs both, start from the load and confirm the forming in a drawing review.
Rolled steel, castings and pipes from one supplier
Many assemblies combine rolled plate, a casting and pipe work, for example a pump base plate in IS 2062, a cast pump casing and IS 1239 pipe lines. Alloynex Foundries, P.No. 17, Bheruji Nagar, Road No. 14, Harmada, Jaipur 302013, supplies rolled steel products, tubes, pipes and fittings, and makes grey iron, SG iron, steel and alloy steel castings to the buyer’s drawing and grade, under ISO 9001, ISO 14001 and ISO 45001. We serve buyers in Jaipur, Ajmer, Kota, Bhilwara, Alwar, Bhiwadi, Neemrana, Jodhpur, Udaipur and across Rajasthan and India. For structural grade choice, see IS 2062 E250 vs E350.
Read next: rolled steel products in Jaipur: a buyer guide, EN 10204 test certificates explained, IS 1239 vs IS 3589 pipe and steel vs alloy steel castings.
FAQs: IS 2062 vs IS 1079
Is IS 1079 steel weaker than IS 2062 steel?
Not weaker by default, but different in purpose. IS 2062 guarantees minimum yield and tensile strength for structural use. IS 1079 grades are chosen for bending, pressing and drawing, so a structural yield value is not the main point of the grade.
Can I use IS 1079 sheet for a welded load-bearing frame?
Usually not. For welded frames, plates and sections that carry load, designers name IS 2062, for example E250 BR or E350 BR. Use IS 1079 for formed sheet parts that do not carry the main structural load.
What do BR, B0 and C mean in IS 2062 grades?
They are impact test levels. BR is tested at room temperature, B0 at 0 °C and C at minus 20 °C. Grade A has no impact test requirement. Pick the level that matches your service temperature and design code.
Which certificate should come with IS 2062 or IS 1079 steel?
Ask for a mill test certificate that shows heat number, chemistry and mechanical results, and name the EN 10204 type, usually 3.1, on your order. Check that the heat number on the paper matches the material.
IS 2062 और IS 1079 में क्या अंतर है?
IS 2062 हॉट रोल्ड स्ट्रक्चरल स्टील का मानक है, जिसमें E250, E350 जैसे ग्रेड न्यूनतम यील्ड और टेंसाइल स्ट्रेंथ की गारंटी देते हैं। IS 1079 हॉट रोल्ड कार्बन स्टील शीट, प्लेट और स्ट्रिप का मानक है, जिसके HR1 से HR4 ग्रेड मोड़ने, प्रेस करने और ड्रॉइंग के लिए चुने जाते हैं।
ढांचे (फ्रेम) के लिए कौन सा स्टील लिखें, IS 2062 या IS 1079?
भार उठाने वाले वेल्डेड फ्रेम, प्लेट और सेक्शन के लिए IS 2062 (जैसे E250 BR या E350 BR) लिखें। प्रेस या मोड़कर बनने वाले शीट पार्ट्स के लिए IS 1079 का उपयुक्त HR ग्रेड लिखें।
Send your drawing for a technical review
Not sure whether your part needs IS 2062 or IS 1079? Send your drawing for a technical review, or request a metallurgy consultation, at info@alloynex.com. See our services.
Last updated: 14 November 2026
Related: IS 2062 and IS 1079 rolled steel for Bhiwadi and Neemrana plants and ERW pipe supplier in Jaipur
Related: IS 2062 plate and MS pipes for Jhunjhunu and Sikar buyers and ASME B16.9 pipe fittings for Sikar and Beawar
IS 2062 vs IS 1079: myths vs facts
Quick answer: IS 2062 is the structural steel standard for plates, sections and bars where strength and weldability are designed in. IS 1079 covers hot rolled carbon steel sheet and strip graded mainly by formability. Choose IS 2062 for load-bearing parts and IS 1079 for pressed, bent or formed sheet parts.
| Myth | Fact |
|---|---|
| “IS 1079 and IS 2062 are the same steel.” | They are different standards: IS 2062 grades (E250, E350…) are set by yield strength; IS 1079 grades (HR1 to HR4) are set mainly by forming quality. |
| “Thicker sheet is always IS 2062.” | The standard depends on the use and product form, not thickness alone. Sheet for pressing is often ordered to IS 1079. |
| “E250 A, BR, B0 and C are just labels.” | The quality letter tells whether an impact test is required and at what temperature. BR, B0 and C carry impact requirements. |
| “Any IS 2062 plate welds the same.” | Carbon equivalent limits differ by grade; state the grade if the part will be welded. |
| “A mill certificate is optional for structural work.” | The certificate ties the plate to its heat chemistry and tensile results; ask for it with every lot. |
Quotable: “IS 2062 for strength you design with; IS 1079 for sheet you form.”
Related: rolled steel by district: quick answers and rolled steel products for Bhilwara buyers.
Next step: Send your drawing for a technical review or request a metallurgy consultation at info@alloynex.com. State grade, size, quantity, tests and delivery town.
Last updated: 15 Nov 2026
What goes wrong when IS 2062 and IS 1079 are mixed up: cause and effect
Short answer: the difference between IS 2062 and IS 1079 is purpose. IS 2062 guarantees strength (and, in BR, B0 and C grades, impact toughness) for load-bearing welded or bolted parts. IS 1079 controls formability for sheet and strip that is bent, pressed or drawn. Using one in place of the other causes predictable problems, shown below.
| Cause (what was ordered) | Where it was used | Effect | Fix on the drawing |
|---|---|---|---|
| IS 1079 HR1 sheet | Welded load-bearing machine base | No guaranteed yield strength; design margin unknown | Specify IS 2062 E250 BR (or higher) for load parts |
| IS 2062 E350 plate | Deep-pressed cover | Cracks or springback in the press | Specify IS 1079 HR3 or HR4 for deep forming |
| “IS 2062” with no grade | Outdoor frame in winter | Grade A supplied with no impact test | Write full grade, for example IS 2062 E250 B0 |
| IS 1079 grade without thickness tolerance check | Press tool set for exact sheet | Uneven forming and scrap | State thickness and tolerance with the grade |
| No certificate named | Any part | Grade cannot be proven at inspection | Ask for mill test certificate or EN 10204 3.1 with heat number |
Rule of thumb: start from the job the steel does. If it carries load, begin with IS 2062 and pick the impact level for the service temperature. If it is mainly shaped, begin with IS 1079 and pick HR1 to HR4 by how hard it is formed. When a part does both, confirm in a drawing review.
See also a worked rolled steel enquiry from Jaipur and rolled steel products for Bhilwara buyers. Send your drawing for a technical review to info@alloynex.com.
Last updated: 15 November 2026
IS 2062 or IS 1079 by part: a specification matrix
Pick the standard from what the part does: if it carries load in a welded or bolted structure, write IS 2062 with a strength grade and impact quality; if it is pressed, bent or drawn sheet that does not carry the main load, write IS 1079 with an HR grade. The matrix below gives a starting line for common parts.
Last updated: 16 Nov 2026
| Part | Standard | Starting grade | Why | Test to ask for |
|---|---|---|---|---|
| Pump or motor base plate | IS 2062 | E250 BR | Welded, carries load, room temperature service | Tensile, impact at room temperature |
| Crane or conveyor frame member | IS 2062 | E350 BR or E350 B0 | Higher yield saves weight; B0 if cold sites | Tensile, impact, chemistry for CE |
| Outdoor structure in cold service | IS 2062 | E250 C or E350 C | Impact tested at -20 °C | Impact at -20 °C |
| Machine guard, cover, panel | IS 1079 | HR1 | Simple bending, no main load | Chemistry, bend |
| Pressed bracket or shallow cup | IS 1079 | HR2 or HR3 | Needs drawing quality to avoid splits | Chemistry, forming trial |
| Deep drawn housing | IS 1079 | HR4 | Extra deep drawing quality | Chemistry, forming trial |
| Flange or pipe support plate | IS 2062 | E250 BR | Bolted joint load | Tensile, impact |
Fact: IS 2062 E250 guarantees a minimum yield strength of 250 MPa and E350 a minimum of 350 MPa (thinner sections).
Fact: IS 2062 impact qualities are BR at room temperature, B0 at 0 °C and C at -20 °C; grade A has no impact test.
Related: बूंदी में पाइप फिटिंग्स सप्लायर · जोधपुर में सीमलेस पाइप सप्लायर · sourcing rolled steel step by step
Request a metallurgy consultation on your part list: info@alloynex.com.