IS 1030 is the Indian Standard for carbon steel castings for general engineering use, and every grade name gives two minimum values in MPa: the 0.2% proof (yield) stress and the tensile strength. For example, IS 1030 Grade 230-450W means at least 230 MPa yield and 450 MPa tensile strength, and the letter W means the grade is meant for welding, with tighter limits on its chemistry.
This guide explains how to read an IS 1030 grade, which grade suits which part, how IS 1030 compares with IS 2644 and ASTM A216 WCB, and how to write the grade correctly on your drawing. It is general education for buyers and engineers. Always check the current BIS edition (IS 1030:1998 is the edition most often cited) and its amendments before you freeze a drawing.
What does an IS 1030 grade name mean?
An IS 1030 grade name has three parts. Read it from left to right and you know the minimum strength and whether the steel is the welding version.
| Part of the name | Example in 230-450W | What it tells you |
|---|---|---|
| First number | 230 | Minimum 0.2% proof (yield) stress in MPa |
| Second number | 450 | Minimum tensile strength in MPa |
| Letter N | (not used here) | Normal grade for general engineering parts |
| Letter W | W | Weldable grade, with tighter limits on carbon and other elements so it can be welded or repaired more safely |
IS 1030 grade table: strength and typical uses
The table below is a reading guide built from the grade names. The strength values are the minimums written into each name. Elongation, reduction of area, impact values and chemistry limits are set in the standard itself, so take them from IS 1030, not from this page.
| IS 1030 grade | Min. 0.2% proof stress (MPa) | Min. tensile strength (MPa) | Versions usually listed | Typical uses (general guidance) |
|---|---|---|---|---|
| 200-400 | 200 | 400 | N and W | Brackets, levers, frames, light covers |
| 230-450 | 230 | 450 | N and W | Machine parts, flanges, housings, general pump and valve parts |
| 270-480 | 270 | 480 | N | Parts that need a little more strength than 230-450 |
| 280-520 | 280 | 520 | N and W | Higher-load machine parts, gear blanks, heavy brackets |
| 340-570 | 340 | 570 | N and W | Wear-prone and highly loaded parts where carbon steel is still enough |
In simple words: as the numbers go up, the steel gets stronger and harder, but it also becomes less forgiving to weld and to machine. Pick the first grade in the table that safely carries your design load, not the strongest one.
N or W: which IS 1030 version should you choose?
Use this decision matrix. If any row on the W side applies to your part, specify the W version.
| Your situation | Choose | Why |
|---|---|---|
| Part will be welded to a pipe, plate or another casting | W | Tighter chemistry lowers the risk of cracks near the weld |
| Foundry may need weld repair of small defects | W | Repair welding is safer on a weldable grade |
| Plain machined part, bolted assembly, no welding | N | N grades meet the strength need without extra limits |
| You are not sure how the part will be joined later | W | It keeps both options open |
| Pressure part working at high temperature | Review the standard | Many buyers specify a pressure-service grade such as ASTM A216 WCB instead |
Glossary: words you will see on an IS 1030 test certificate
- 0.2% proof stress: the stress at which the steel has taken a small permanent stretch of 0.2%. It is used as the yield value for castings.
- Tensile strength: the highest stress the test bar carries before it breaks.
- Elongation: how much the test bar stretches, in percent, before it breaks. Higher means more ductile.
- Charpy impact energy: the energy, in joules, needed to break a notched sample. It shows toughness, often at a set temperature.
- Heat number: the batch code of one melt. It links the castings, the test bars and the certificate.
- Normalising: heating above the critical range and cooling in air to refine the grain. Most steel castings are supplied heat treated.
- EN 10204 3.1: a certificate type where the results come from the actual heat and are signed by the maker’s inspection staff, independent of production.
IS 1030 vs IS 2644 vs ASTM A216 WCB: what is the difference?
IS 1030 covers carbon steel castings for general engineering. IS 2644 covers high tensile steel castings, which are usually low alloy steels heat treated to much higher strength. ASTM A216 WCB is an American carbon steel grade for pressure-containing parts such as valve bodies and flanges at high temperature.
| Point | IS 1030 | IS 2644 | ASTM A216 WCB |
|---|---|---|---|
| Steel type | Carbon steel | High tensile, usually low alloy steel | Carbon steel |
| Main use | General engineering castings | Highly stressed parts | Valves, flanges, fittings for pressure and high-temperature service |
| How grades are named | Yield-tensile in MPa plus N or W (for example 230-450W) | CS plus minimum tensile in MPa (for example CS 640, CS 840) | Letter code (WCA, WCB, WCC) |
| Example minimums | 230-450W: 230 yield, 450 tensile | CS 640: 640 tensile | WCB: 250 yield, 485 tensile |
| Usual supply condition | Heat treated as the standard or order states, often normalised | Heat treated to reach the grade, often hardened and tempered | Annealed, normalised, or normalised and tempered |
Watch out for one common mix-up: IS 2644 has a grade called CS 1030. That is a high tensile grade with a minimum tensile strength of 1030 MPa. It is not the same thing as a casting to IS 1030. Always write both the standard and the grade.
How to specify an IS 1030 casting on a drawing: a worked example
Say you need a pump bracket that carries a moderate load and will be welded to a base frame. Follow these steps.
- Pick the strength level. Your design needs about 230 MPa yield, so choose the 230-450 grade.
- Pick N or W. The bracket will be welded, so choose 230-450W.
- State the heat-treatment condition. Write “normalised” (or the condition your design needs) so the foundry and the certificate match.
- List the tests. Chemical analysis, tensile test (yield, tensile, elongation) and hardness. Add Charpy impact only if toughness at a set temperature matters.
- Ask for the certificate. EN 10204 type 3.1, traceable by heat number.
- Add tolerances and allowances. Name the ISO 8062-3 tolerance grade and the machining allowance on machined faces.
- Mark critical zones. Show where defects are not acceptable, such as bolt bosses and weld edges, and any inspection your design needs there.
The finished material note in the title block can look like this:
MATERIAL: STEEL CASTING TO IS 1030, GRADE 230-450W CONDITION: NORMALISED TESTS: CHEMICAL, TENSILE (YIELD, UTS, ELONGATION), HARDNESS CERTIFICATE: EN 10204 TYPE 3.1, HEAT NUMBER TRACEABLE TOLERANCE: ISO 8062-3 DCTG AS PER DRAWING, RMA ON MACHINED FACES CRITICAL ZONES: AS MARKED, NO WELD REPAIR WITHOUT APPROVAL
How Alloynex handles IS 1030 steel casting enquiries
Alloynex Foundries in Harmada, Jaipur, makes steel and alloy steel castings to the buyer’s drawing and grade, under ISO 9001, ISO 14001 and ISO 45001 systems. Our engineers review the grade, the heat-treatment condition and the test list on every drawing before we reply. Read more about steel vs alloy steel castings, normalizing vs annealing steel castings, EN 10204 test certificates and machining allowance on castings, or see our casting services.
FAQs
What is the difference between IS 1030 200-400W and 230-450W?
Both are weldable carbon steel casting grades. 200-400W has a minimum of 200 MPa yield and 400 MPa tensile, while 230-450W has a minimum of 230 MPa yield and 450 MPa tensile, so it suits parts that carry more load.
Is IS 1030 the same as ASTM A216 WCB?
No. They are close in strength but are different standards with different chemistry, test and marking rules. WCB is written for pressure parts at high temperature. Do not swap one for the other without your design engineer’s approval.
Which IS 1030 grade is common for machine parts?
230-450 is the most common general choice. Use 280-520 where the load is higher, and the W version of either when the part will be welded.
IS 1030 में 230-450W का क्या मतलब है?
230-450W का मतलब है कम से कम 230 MPa यील्ड (0.2% प्रूफ स्ट्रेस) और 450 MPa टेन्साइल स्ट्रेंथ। W का मतलब है कि यह वेल्डिंग के लिए बना ग्रेड है, जिसकी केमिस्ट्री पर सख़्त सीमा होती है।
IS 1030 और IS 2644 में क्या अंतर है?
IS 1030 सामान्य इंजीनियरिंग के लिए कार्बन स्टील कास्टिंग का मानक है। IS 2644 हाई टेन्साइल स्टील कास्टिंग का मानक है, जिसके ग्रेड CS 640, CS 840 जैसे नाम से आते हैं। IS 2644 का CS 1030 ग्रेड, IS 1030 नहीं है।
Send your drawing for a technical review
Share your drawing, IS 1030 grade (or the grade you are considering), weight, quantity and required tests at info@alloynex.com. Not sure which grade fits? Request a metallurgy consultation at the same address and our engineers will review the part with you.
Last updated: 14 November 2026
Related: IS 1030 steel castings for Bhiwadi and Neemrana buyers
Related: alloy steel castings for Kishangarh and Ajmer: grades, tests and RFQ checklist
Related: IS 1030 steel castings for Sirohi and Abu Road buyers
Related: IS 1030 and alloy steel castings for Sikar and Beawar buyers
Related: rolled steel bar or plate instead of a casting: grades for Kotputli-Behror plants
Related: IS 1030 steel castings for Didwana-Kuchaman and Makrana buyers, SG iron castings for Bharatpur, IS 210 grey iron castings for Tonk and Jaisalmer and seamless steel tubes for Jodhpur.
IS 1030 grade step selector: 200-400W, 230-450W, 280-520W or 340-570W?
Answer the questions in order and stop at the first “yes”. The result is a starting grade for the drawing review, not a final design check. Last updated: 15 Nov 2026
| Step | Question | If yes, start with | Minimum yield / tensile (MPa) |
|---|---|---|---|
| 1 | Is the part high load, with wear, and no welding planned? | 340-570N | 340 / 570 |
| 2 | Is the part high load and will it be welded or weld repaired? | 280-520W | 280 / 520 |
| 3 | Is it a general machine part under moderate load (brackets, housings, levers)? | 230-450W | 230 / 450 |
| 4 | Is it a light-load part where weldability and machining ease matter most? | 200-400W | 200 / 400 |
| 5 | Is it a pressure part at high temperature, or does the code name ASTM? | Keep the ASTM grade (for example A216 WCB) on the drawing | Per that standard |
After the grade, add the condition (normalised, or normalised and tempered), the tests and the certificate type, then send the drawing for a technical review.
Related: pipe fittings for Balotra and Barmer · grey iron castings for Deeg · ERW pipe for Bundi · SG iron pump castings for Phalodi.
Who supplies steel castings to buyers in Tonk?
Answer: Alloynex Foundries, Harmada, Jaipur, makes carbon steel and alloy steel castings to drawing for buyers in Tonk, Newai, Niwai, Malpura, Deoli and Uniara. Most Tonk machine parts are ordered in IS 1030 grades such as 230-450W, normalized. Send your drawing to info@alloynex.com for a technical review.
Steel casting specs for common Tonk parts
| Part (typical Tonk use) | Starting grade | Condition | Tests to ask for |
|---|---|---|---|
| Machine frames, levers, brackets (stone and mineral units) | IS 1030 230-450W | Normalized | Chemistry, tensile, elongation, hardness |
| Gear blanks, hubs, couplings | IS 1030 280-520N | Normalized, or normalized and tempered | Above plus hardness on the working face |
| Crusher and grinder wear parts | Austenitic manganese steel (IS 276) or alloy steel | As the grade requires | Chemistry, hardness, visual |
| Valve bodies and flanges for water lines | IS 1030 230-450W, or ASTM A216 WCB if your spec names it | Normalized | Above plus pressure test |
How to choose and order: 6 steps
- Write the duty: load, shock, wear, heat and whether the part is welded.
- Pick the first IS 1030 grade in the table above that carries the load; choose the W version if it will be welded.
- Move to alloy steel or manganese steel only if wear or heat demands it.
- Name the heat treatment condition, usually normalized.
- Mark machined faces and add an ISO 8062-3 tolerance and allowance note.
- List the tests and ask for an EN 10204 3.1 certificate tied to the heat number.
Steel vs SG iron vs grey iron castings for Tonk buyers
| Point | Steel casting (IS 1030) | SG iron (IS 1865) | Grey iron (IS 210) |
|---|---|---|---|
| Shock and impact | Very good | Good | Poor |
| Welding | Yes (W grades) | Limited | Not advised |
| Vibration damping | Low | Medium | High |
| Typical parts | Levers, frames, valve bodies | Housings, hubs, pump bodies | Machine beds, covers, pulleys |
FAQs: steel castings for Tonk
Which IS 1030 grade suits most Tonk machine parts?
IS 1030 230-450W is the usual start for frames, levers and brackets. Use 280-520N where the load is higher and welding is not needed.
Do steel castings come with a test certificate?
Ask for an EN 10204 3.1 certificate showing chemistry, tensile, elongation and hardness, linked to the heat number and heat treatment.
टोंक में स्टील कास्टिंग कौन सप्लाई करता है?
एलॉयनेक्स फाउंड्रीज़, हरमाड़ा, जयपुर, ड्रॉइंग के अनुसार कार्बन स्टील और अलॉय स्टील कास्टिंग बनाती है और टोंक, निवाई, मालपुरा और देवली के खरीदारों को सप्लाई करती है। ड्रॉइंग info@alloynex.com पर भेजें।
स्टील कास्टिंग और SG आयरन कास्टिंग में क्या अंतर है?
स्टील कास्टिंग झटका सहने और वेल्डिंग के लिए बेहतर है। SG आयरन कास्टिंग हाउसिंग और पंप बॉडी जैसे पार्ट्स के लिए आम है, जहाँ मशीनिंग आसान चाहिए।
Read next: a worked steel casting example from Abu Road, steel vs alloy steel castings and EN 10204 certificates explained. Send your drawing for a technical review to info@alloynex.com.
Last updated: 15 November 2026
Related: SG iron castings for hydraulic cylinders and valves for Bhiwadi OEMs, compressor body and cylinder castings in Jaipur, झुंझुनू में पाइप फिटिंग्स और फ्लैंज सप्लायर and राजस्थान में कास्टिंग सप्लायर: हिंदी गाइड.
IS 1030 grade 280-520W explained: quick answer, myths and facts
Quick answer: IS 1030 grade 280-520W is a weldable carbon steel casting grade with a minimum 0.2% proof stress of 280 MPa and a minimum tensile strength of 520 MPa. The W means tighter chemistry limits so the casting can be welded or weld repaired. It suits higher-load brackets, frames, crusher and pump parts that will be welded. Last updated: 16 Nov 2026
| Myth | Fact |
|---|---|
| 280-520W is just a stronger 230-450W. | It is stronger, but the W version also limits carbon and other elements so the steel stays weldable. Check both strength and weldability. |
| W and N versions have the same chemistry. | No. The N version is not intended for welding. If any welding or weld repair is planned, write W on the drawing. |
| The numbers are typical values. | They are minimums: 280 MPa proof stress and 520 MPa tensile on test bars from the same heat. |
| Hardness alone proves the grade. | Hardness is a quick check only. The grade is proven by chemical analysis and a tensile test, reported on an EN 10204 3.1 certificate. |
| Any carbon steel casting can be swapped for ASTM A216 WCB. | No. WCB is a pressure-part grade with its own rules. Keep the grade the designer named. |
IS 1030 280-520W quick card
| Item | 280-520W |
|---|---|
| Min. 0.2% proof stress | 280 MPa |
| Min. tensile strength | 520 MPa |
| Weldable version | Yes (W) |
| Usual condition | Normalised, or normalised and tempered |
| Typical parts | Load-carrying brackets, frames, levers, crusher and pump parts that will be welded |
| Tests to ask for | Chemistry per heat, tensile, hardness, dimensional report |
| Certificate | EN 10204 3.1 linked by heat number |
हिंदी में त्वरित उत्तर: IS 1030 280-520W क्या है?
IS 1030 ग्रेड 280-520W एक वेल्ड होने वाला कार्बन स्टील कास्टिंग ग्रेड है। इसमें कम से कम 280 MPa प्रूफ स्ट्रेस और 520 MPa टेन्साइल स्ट्रेंथ होती है। ज़्यादा लोड वाले ब्रैकेट, फ्रेम और पंप पार्ट्स के लिए, जिन पर वेल्डिंग होनी है, यह ग्रेड चुना जाता है।
Alloynex Foundries, Harmada, Jaipur, makes steel castings to the buyer’s drawing for plants across Rajasthan. Name the IS 1030 grade on the drawing. Related: cement plant wear-part castings for Beawar and EN 10204 test certificates. Send your drawing for a technical review to info@alloynex.com, or request a metallurgy consultation on the grade.