Ductile iron castings in Jodhpur are best ordered by IS 1865 grade: SG 400/15 or SG 400/18 for parts that must bend without cracking, and SG 500/7 for parts that need more strength. Alloynex Foundries in Jaipur makes ductile (SG) iron castings to drawing and supplies buyers across Jodhpur and western Rajasthan.
Last updated: 20 November 2026
Grey iron castings for Jodhpur buyers: quick facts
Alloynex Foundries, Harmada, Jaipur, makes grey iron and SG iron castings to the buyer’s drawing for plants in Jodhpur, Pali, Balotra and Barmer. Name the IS 210 grade (for example FG 200 or FG 260) on the drawing, and ask for the chemical and tensile results you need with each lot. Send the drawing to info@alloynex.com.
| Item | Detail |
|---|---|
| Firm | Alloynex Foundries |
| Location | Harmada, Jaipur, Rajasthan |
| Products | Grey iron, SG iron, steel and alloy steel castings to drawing |
| Quality system | ISO 9001, ISO 14001, ISO 45001 |
| Buyers served | Jodhpur, Pali, Balotra, Barmer |
| Grade to ask for | Name the IS 210 grade on the drawing (for example FG 200 or FG 260) |
| Documents to ask for | Chemical and tensile results for each lot, as agreed at order |
| Contact | info@alloynex.com |
Start in 3 steps:
- Mark the IS 210 grade, weight and quantity on the drawing.
- List the tests and documents you want to ask for.
- Send the drawing to info@alloynex.com for a technical review.
This guide explains IS 1865 grades in simple words, what SG 500/7 really means, how to pick a grade and which tests to ask for. It is written for design engineers, QA heads and buyers in Jodhpur.
Ductile iron castings for Jodhpur industry
Jodhpur has a strong base of engineering units in Basni, Boranada, Marudhar Industrial Area and Sangariya. Pump and valve makers, mining and stone-cutting machine builders, farm equipment makers and process plants all use iron castings.
Many of these parts work under shock, vibration or pressure. Grey iron cracks without warning under such loads because its graphite is in flakes. Ductile iron has graphite in round nodules, so it can stretch before it breaks. That one change gives two to three times the strength of common grey iron grades.
Ductile iron, SG iron and nodular iron are the same material. In India the standard is IS 1865. In Europe it is EN 1563 (for example EN-GJS-500-7), and in the USA it is ASTM A536.
IS 1865 grades at a glance
Each IS 1865 grade name gives two numbers: minimum tensile strength in MPa and minimum elongation in percent. SG 500/7 means 500 MPa and 7%.
| IS 1865 grade | Min. tensile strength | Min. 0.2% proof stress | Min. elongation | Main matrix |
|---|---|---|---|---|
| SG 350/22 | 350 MPa | 220 MPa | 22% | Ferrite |
| SG 400/18 | 400 MPa | 250 MPa | 18% | Ferrite |
| SG 400/15 | 400 MPa | 250 MPa | 15% | Ferrite |
| SG 450/10 | 450 MPa | 310 MPa | 10% | Ferrite |
| SG 500/7 | 500 MPa | 320 MPa | 7% | Ferrite and pearlite |
| SG 600/3 | 600 MPa | 370 MPa | 3% | Pearlite and ferrite |
| SG 700/2 | 700 MPa | 420 MPa | 2% | Pearlite |
| SG 800/2 | 800 MPa | 480 MPa | 2% | Pearlite or tempered structure |
| SG 900/2 | 900 MPa | 600 MPa | 2% | Tempered martensite |
Values are minimums on separately cast test samples, as published in IS 1865. As strength goes up, elongation goes down. Pick the first grade in the table that meets your load, because softer grades machine more easily and resist shock better.
SG 500/7 properties explained
SG 500/7 is the most widely ordered ductile iron grade. It sits in the middle of the range and suits housings, brackets, hubs, gear blanks, pump casings and machine parts.
- Tensile strength: 500 MPa minimum.
- 0.2% proof stress: 320 MPa minimum.
- Elongation: 7% minimum.
- Typical hardness: about 170 to 230 HB (informative range given in EN 1563 for EN-GJS-500-7).
- Density: about 7.1 g/cm³, a little lower than steel.
- Matrix: a mix of ferrite and pearlite, usually reached as-cast without heat treatment.
Compared with FG 260 grey iron, SG 500/7 has almost twice the tensile strength and real elongation, but slightly lower vibration damping. Read our full comparison of SG iron vs grey cast iron.
How to choose the right grade: five steps
- Define the load. Write the main load, any shock, the pressure and the working temperature.
- Decide if ductility matters most. For pressure parts and parts that see impact, start with SG 400/15 or SG 400/18.
- Decide if strength matters most. For housings and machine parts, SG 500/7 is the usual start. For gears and wear parts, look at SG 600/3 or SG 700/2.
- Check heat treatment. Ferritic grades may need annealing; higher grades may need normalising. See our guide on heat treatment of castings.
- Write it on the drawing. For example: SG iron SG 500/7 to IS 1865, minimum nodularity agreed, EN 10204 3.1 certificate. Add machining allowance as per our guide on machining allowance on castings.
| Part type | Starting grade | Why |
|---|---|---|
| Pump and valve bodies | SG 400/15 or SG 400/18 | High elongation, good for pressure |
| Housings, brackets, hubs | SG 500/7 | Balance of strength and ductility |
| Gears, sprockets, rollers | SG 600/3 or SG 700/2 | Higher strength and wear life |
| Parts under impact at low temperature | SG 400/18 with impact test | Best toughness |
Tests and certificates to ask for
A grade on paper means little without tests. For ductile iron castings, ask for these checks on each heat or lot:
- Tensile test for tensile strength, 0.2% proof stress and elongation.
- Hardness test in Brinell (HB) on the casting or test piece.
- Chemical analysis of carbon, silicon, manganese, sulphur, phosphorus and magnesium.
- Microstructure for nodularity and matrix. Many buyers set a minimum nodularity, often 80% or more.
- Visual and dimensional check against the drawing, with NDT where the part is critical.
Ask for results on an EN 10204 type 3.1 certificate. Our guide on EN 10204 test certificates shows how to read one. For a full ordering list, see our castings buyer guide for Rajasthan.
FAQs
What is the difference between ductile iron and SG iron?
There is no difference. Ductile iron, SG iron (spheroidal graphite iron) and nodular iron are three names for the same material. In India it is covered by IS 1865.
What are the properties of SG 500/7?
SG 500/7 to IS 1865 has a minimum tensile strength of 500 MPa, a minimum 0.2% proof stress of 320 MPa and a minimum elongation of 7%. Its matrix is ferrite plus pearlite, and typical hardness is about 170 to 230 HB.
Which IS 1865 grade is used for pump and valve bodies?
SG 400/15 and SG 400/18 are common for pressure parts that need high ductility. SG 500/7 is common where more strength is needed with fair ductility, such as housings and brackets.
What tests should come with ductile iron castings?
Ask for a tensile test with proof stress and elongation, hardness, chemical analysis and a nodularity check by microscope, reported on an EN 10204 3.1 certificate for each heat or lot.
Does Alloynex supply ductile iron castings to Jodhpur?
Yes. Alloynex Foundries, Jaipur, makes SG iron castings to drawing for buyers in Jodhpur, including Basni, Boranada, Marudhar Industrial Area and Sangariya. Send your drawing for a technical review to info@alloynex.com.
जोधपुर के खरीदारों के लिए डक्टाइल आयरन: हिंदी में सवाल-जवाब
डक्टाइल आयरन और SG आयरन में क्या अंतर है?
कोई अंतर नहीं है। डक्टाइल आयरन, SG आयरन और नोड्यूलर आयरन एक ही मटेरियल के नाम हैं। भारत में इसका स्टैंडर्ड IS 1865 है।
SG 500/7 का क्या मतलब है?
SG 500/7 का मतलब है न्यूनतम तन्यता 500 MPa और न्यूनतम एलोंगेशन 7%। इसका प्रूफ स्ट्रेस कम से कम 320 MPa होता है। हाउसिंग, ब्रैकेट और हब जैसे पार्ट के लिए यह आम ग्रेड है।
जोधपुर में डक्टाइल आयरन कास्टिंग कहाँ से लें?
Alloynex Foundries, जयपुर, ड्रॉइंग के अनुसार SG आयरन कास्टिंग बनाती है और जोधपुर सहित पूरे राजस्थान में भेजती है। अपनी ड्रॉइंग info@alloynex.com पर भेजें।
Send your drawing for a technical review. Email your drawing, IS 1865 grade, yearly quantity and test needs to info@alloynex.com, or request a metallurgy consultation. Alloynex Foundries, P. No. 17, Bheru ji Nagar, Road No. 14, Harmada, Jaipur, Rajasthan 302013, works to ISO 9001, ISO 14001 and ISO 45001 systems.
Related: shrinkage porosity vs gas porosity in ductile iron castings
Also read: SG iron vs grey iron for pump and valve bodies in Nagaur and Bharatpur and castings for Banswara, Dungarpur and Pratapgarh
Related: SG iron castings for Sikar and Churu buyers
Related: SG 400/15 and SG 500/7 property table for Nagaur and Sirohi buyers
Related: ductile iron castings for Udaipur and Rajsamand buyers and SG iron castings supplier for Chittorgarh
Related: SG (ductile) iron castings for Jalore, Bhinmal and Sanchore buyers
Ductile iron glossary for Jodhpur buyers: 12 terms explained
Short answer: most questions on a Jodhpur ductile iron order come down to twelve words: nodularity, nodule count, ferrite, pearlite, proof stress, elongation, test bar, magnesium treatment, inoculation, carbide, shrinkage and Brinell hardness. Knowing them helps buyers in Basni, Boranada, Phalodi and Balotra read an IS 1865 test certificate and compare suppliers fairly.
- Nodularity: the share of graphite that is round. Buyers usually ask for 80% or more; low nodularity lowers strength and elongation.
- Nodule count: the number of graphite nodules per square millimetre. A higher count usually means a finer, sounder structure.
- Ferrite: the soft, ductile part of the matrix. Ferritic grades such as SG 400/15 and SG 400/18 bend before they break.
- Pearlite: the stronger, harder part of the matrix. Pearlitic grades such as SG 600/3 and SG 700/2 resist wear.
- 0.2% proof stress: the stress at which the metal starts to stretch permanently. IS 1865 gives a minimum for each grade, for example 320 MPa for SG 500/7.
- Elongation: how much a test bar stretches before it breaks, in percent. It is the second number in the grade name.
- Test bar: a sample cast with the heat, either separately cast or cast-on, used for the tensile test.
- Magnesium treatment: the step that turns graphite from flakes into nodules. Without it, the metal stays grey iron.
- Inoculation: a late addition, usually ferrosilicon, that raises nodule count and prevents hard carbides.
- Carbide (chill): very hard iron carbide in thin sections. It makes machining difficult and can be removed by annealing.
- Shrinkage: voids that form when thick sections cool last. Good feeding and casting design prevent it.
- Brinell hardness (HB): a hardness number from a ball impression, tested to IS 1500. SG 500/7 is typically about 170 to 230 HB.
Want these checked on your part? Request a metallurgy consultation at info@alloynex.com.
Related: SG iron castings for Jhalawar and Kota buyers and ductile iron order sheet for Udaipur buyers.
Last updated: 15 Nov 2026
Who supplies SG iron castings to buyers in Boranada, Jodhpur?
Answer: ALLOYNEX FOUNDRIES, Jaipur, makes SG (ductile) iron castings to drawing for engineering units in Boranada, Basni and other Jodhpur industrial areas. Typical grades are IS 1865 SG 400/15, 450/10, 500/7 and 600/3. Send your drawing to info@alloynex.com for a technical review.
SG iron grade table for Boranada buyers (IS 1865)
| IS 1865 grade | Min tensile (MPa) | Min elongation (%) | Typical Boranada use |
|---|---|---|---|
| SG 400/15 | 400 | 15 | Pump and valve bodies needing toughness |
| SG 450/10 | 450 | 10 | Housings, brackets, pipe fittings bodies |
| SG 500/7 | 500 | 7 | Gear blanks, pulleys, machine parts |
| SG 600/3 | 600 | 3 | Wear-loaded parts, hubs, rollers |
How to order SG iron castings from Boranada in 5 steps
- Send the drawing (PDF or DWG) with part weight and annual quantity.
- State the grade, e.g. IS 1865 SG 500/7, or the equivalent ISO 1083 / ASTM A536 grade your customer uses.
- List tests: chemistry, tensile, hardness and nodularity (microstructure) if the part is critical.
- Give the tolerance grade (ISO 8062-3 DCTG) and machining allowance.
- Name the delivery point in Boranada or elsewhere in Jodhpur and the certificate you need (EN 10204 2.2 or 3.1).
SG iron vs grey iron vs cast steel for Jodhpur parts
| Need | SG iron (IS 1865) | Grey iron (IS 210) | Cast steel (IS 1030) |
|---|---|---|---|
| Impact and shock | Good | Poor | Very good |
| Vibration damping | Medium | Very good | Low |
| Weldability | Limited | Poor | Good |
| Machinability | Good | Very good | Fair |
| Typical parts | Pump casings, valve bodies, brackets | Machine beds, covers, pulleys | High-pressure valve bodies, heavy-duty brackets |
Quotable: “SG iron gives grey-iron castability with near-steel toughness; IS 1865 SG 500/7 is the common general-engineering grade.” “Ask for nodularity results when an SG iron part carries shock load.”
FAQs
Which SG iron grade suits pump bodies made for Boranada units?
IS 1865 SG 400/15 or SG 450/10 is usual where toughness matters; confirm with your design pressure and drawing.
Can I ask for a 3.1 certificate for SG iron castings in Jodhpur?
State the certificate type you need, such as EN 10204 3.1, in the RFQ; it is reviewed with the drawing.
बोरानाडा, जोधपुर के लिए एसजी आयरन कास्टिंग कौन बनाता है?
ALLOYNEX FOUNDRIES, जयपुर, ड्रॉइंग के अनुसार एसजी आयरन कास्टिंग बनाती है। ड्रॉइंग पर IS 1865 ग्रेड (जैसे SG 500/7) लिखें। ड्रॉइंग info@alloynex.com पर भेजें।
एसजी आयरन और ग्रे आयरन में क्या फर्क है?
एसजी आयरन में ग्रेफाइट गोल (नोड्यूल) होता है, इसलिए यह मजबूत और कम भंगुर है; ग्रे आयरन में ग्रेफाइट परतदार होता है जो कंपन सोखता है।
Related: SG iron vs grey cast iron · pipe fittings for Basni, Jodhpur
Next step: Send your drawing for a technical review or request a metallurgy consultation at info@alloynex.com. State grade, size, quantity, tests and delivery town.
Last updated: 15 Nov 2026
Ductile iron castings in Jodhpur: cause and effect of common problems
Short answer: most ductile iron (SG iron) problems seen by Jodhpur pump, valve and machine builders trace back to four causes: poor nodularity, the wrong matrix for the grade, shrinkage in thick sections, and missing test proof. Each cause has a clear effect in service and a simple check you can ask for at the enquiry stage.
| Cause | Effect you see | Check to ask for |
|---|---|---|
| Low nodularity (graphite not round enough) | Low elongation; part cracks under shock like grey iron | Nodularity report by microscope for each heat or lot |
| Too much pearlite in SG 400/15 or 400/18 | Hardness too high; poor ductility in pressure parts | Hardness test plus microstructure photo |
| Too much ferrite in SG 500/7 or 600/3 | Strength below grade; wear on hubs and gear blanks | Tensile test with 0.2% proof stress |
| Shrinkage in thick bosses or flanges | Leaks in pump and valve bodies after machining | Feeding plan review; pressure test where needed |
| Chemistry drift (magnesium fade) | Mixed graphite shapes in late pours | Chemical analysis tied to heat number |
| No traceable certificate | Disputes at incoming inspection | EN 10204 3.1 certificate with heat number |
How to use this table: read the “effect” column first. If you have seen that problem on an earlier lot from Basni, Boranada or Marudhar Industrial Area suppliers, add the matching check to your drawing note. For example: “IS 1865 SG 500/7; nodularity min. as agreed; tensile, proof stress, elongation and hardness on EN 10204 3.1.”
For defect causes in more depth, read common casting defects and how foundries prevent them. To compare materials first, see SG iron vs grey cast iron.
Send your drawing for a technical review to info@alloynex.com. Alloynex Foundries, P.No. 17, Bheruji Nagar, Road No. 14, Harmada, Jaipur 302013.
Last updated: 15 November 2026
Ductile iron castings in Jodhpur: defect, cause and remedy table
Most rejections of IS 1865 ductile iron castings come from six defects: low nodularity, shrinkage porosity, gas holes, carbides at thin edges, low elongation and cracks. Each one has a known cause in the melt or the mould, and each can be caught by a test that Jodhpur buyers can ask for on the certificate.
Last updated: 16 Nov 2026
| Defect seen | Likely cause | Remedy at the foundry | What the buyer checks |
|---|---|---|---|
| Low nodularity, low strength | Magnesium faded, high sulphur, long hold after treatment | Control sulphur, pour within the fade time, inoculate | Nodularity report from the microscope |
| Shrinkage porosity at thick bosses | Hot spot not fed, wrong riser or chill | Simulation, risers or chills on heavy sections | Cut section or X-ray on first article |
| Gas holes under the skin | Wet sand, high moisture cores, slag | Sand control, dry cores, clean ladles | Visual after shot blasting and machining |
| Hard edges, poor machining | Carbides in thin sections, low inoculation | Late inoculation, section design | Hardness at thin walls |
| Elongation below grade, e.g. under 7% for SG 500/7 | Too much pearlite or carbides | Chemistry control, ferritizing anneal if needed | Tensile report with elongation |
| Cracks at section changes | Sharp corners, early knockout | Fillets on the drawing, controlled cooling | Dye penetrant or MPI on critical areas |
Fact: IS 1865 SG 500/7 needs at least 500 MPa tensile strength, 320 MPa proof stress and 7% elongation.
Fact: nodularity is usually checked on a polished sample at 100x magnification and reported as a percentage.
Related: जोधपुर में सीमलेस पाइप सप्लायर · FG 260 grey iron castings for Sikar · marble machinery castings in Kishangarh
Seeing one of these defects on a current supply? Send the drawing and photos for a technical review: info@alloynex.com.